52H Glass Sealing52 Vacodil 520 Wire 0.5mm and 0.8mm large in stock with fast delivery
Chemical Composition
Grade | C% | P% | S% | Mn% | Si% | Cu% | Cr% | Mo% | Ni% | Co% | Fe% |
Alloy52 | Max 0.05 | Max 0.020 | Max 0.020 | Max 0.80 | Max 0.30 | / | / | / | 51.5~52.5 | / | Bal. |
Specifications
Grade | Common Name | Common Name |
Alloy52 | Vacodil520 | NILO 52 |
Physical Properties
Grade | Density | Resistivity |
Alloy52 | 8.25 g/cm3 | 0.43 |
Grain size of Alloy52
The grain size of the alloy deep-drawing belt should not be less
than level 7, and the grain size less than level 7 should not
exceed 10% of the area. When the average grain size of the strip
with a thickness of less than 0.13mm is estimated, the number of
grains along the thickness of the strip should be no less than 8.
Welding performance of Alloy52
The combined gold has good welding performance and can be brazed
and spot welded. The combination of gold and soft glass should be
pre-oxidized before sealing.
Coefficient of Expansion
Alloy | Linear Coefficient of Thermal Expansion a,10-6/°C | |||||||
20-200°C | 20-300°C | 20-350°C | 20-450°C | 20-500°C | 20-600°C | 20-700°C | 20-800°C | |
Kovar | 10.4 | 10.2 | 10.3 | 10.3 | 10.3 | 10.8 | / | / |
Heat Treatment For Alloy52
(1) Stress relief annealing In order to eliminate the residual
stress of parts after machining, stress relief annealing is
required: 430~540℃, heat preservation 1~2h, furnace cooling or air
cooling. [1]
(2) Intermediate annealing In order to eliminate the work hardening
phenomenon caused by the alloy in the process of cold rolling, cold
drawing and cold stamping, in order to facilitate the continued
processing. The workpiece needs to be heated to 700~800℃ in a
vacuum or protective atmosphere for 30~60min, then furnace cooled,
air cooled or water quenched.
(3) Pre-oxidation treatment When the combined gold is used as a
sealing material, it should be pre-oxidized before sealing. A
uniform and dense oxide film is formed on the surface of the alloy.
The parts are heated in saturated wet hydrogen at 1100°C for 30
minutes, and then oxidized in the air at about 800°C for 5-10
minutes. The weight gain of the parts should be 0.1~0.3mg/cm2
Ohmalloy Material Co.,Ltd
Ohmalloy Material Co.,Ltd is a high-tech enterprise which specialized in making all kinds of alloy such as high resistance alloy, low-resistance copper nickel alloy, precision alloy, FeCrAl alloy and thermocouple Alloy.
Ohmalloy Material Co.,Ltd have a full production line from melting, surface cleaning, rolling and slitting, full set of testing machine and can meet all kinds of technical requirement from customer. Our product is widely used in heating equipment, big steel mill, mineral, electrical equipment, food machinery, auto industry, aerospace industry. Our product not only is popular in domestic market, but also been exported to all over the world.
Our company aims to be the best-quality alloy producer in the
world. We insist on developing the more advanced alloy strip
technology, to serve all the customer, improve people’s living