Home /

High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic

Send your message to this supplier
*From:
Your email address is incorrect!
To:Shanghai Tankii Alloy Material Co.,Ltd
*Subject:
Your subject must be between 10-255 characters!
*Message:
Your message must be between 20-3,000 characters!
Yes!I would like your verified suppliers matching service!
Buy cheap High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic Regenerator from wholesalers
  • Buy cheap High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic Regenerator from wholesalers
  • Buy cheap High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic Regenerator from wholesalers

High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic Regenerator

Ask Latest Price
Brand Name:TANKII
Certification:COO, CCPIT
Price:negotiation
Payment Terms:Ex works/ FOB/ CPT
Supply Ability:30,000 kgs/ month
Delivery Time:25-30 days
Model Number:GH3600
MOQ:50kg
Company Data
Verified Supplier
Contact Person Martin Lee
Business Type: Manufacturer Exporter
Officials: 1900 Mudanjiang Road, Baoshan District, 201999, Shanghai, China
Quality: Quality Certifitation Available
Visit Website
Product Details Company Profile
Product Details

High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic Regenerator


Quick Detail:


Name

Inconel 600

UNS N06600

GH3600


Application

thermowell work in Erosion atmosphere; Anti-chlorine, hydrogen chloride, oxidation and carbonization corrosion; Nuclear reactor

Condition

Bright/ Oxidized

Soft/ Hard

Feature

GH3600 for a variety of corrosive media have corrosion resistance.

Petrochemical production of catalytic regenerator over 700 ℃ applications alloy 600 is recommended for longer life.

Shape

Strip, Foil, Sheet, Wire, Bar.

Standard



Description:


Chemical composition(%)


Grade

C

Si

Mn

P

S

Ni

Cr

Cu

Fe

GH3600

≤0.15

≤0.5

≤ 1

≤0.015

≤0.015

72

14~17

≤0.5

6~7


Physical properties

>Density (g/cm3): 8.4

>Melting point (℃): 1370~1425


Mechanical properties



Yield Strength (Mpa)

Tensile Strength (Mpa)

Elongation, %

Hardness, HB

GH3600

Cold-rolling

240

550

30

≤195

As annealed

180

500

35

≤185


Specifications

Grade

GH3600

Size

Ф 0.1~20mm

MOQ

50 kgs

Condition

Soft/ Hard; Bright/ Oxidized

High Temp Alloy Superalloy- GH3600 ( Inconel 600 ) for Thermowell , Catalytic Regenerator

Company Profile

Shanghai Tankii Alloy Material Co.,Ltd

Shanghai Tankii Alloy Material Co., Ltd.specialized in production of Resistance Heating Alloy, Nickel Chromium Alloy, Iron Chromium Aluminum Alloy, Nickel Aluminum Alloy, Manganin, Copper Nickel Alloy, thermocouple wire, pure nickel and other precision alloy materials in the form of round wire, ribbon wire, sheet, tape, strip, rod and plate.

 

We’ve already got ISO9001 quality system certificate and approval of ISO14001 environmental protection system.

We own a complete set of advanced production flow of refining, cold reduction, drawing and heat treating etc. We also proudly have independent R&D capacity.

 

Shanghai Tankii Alloy Material Co., Ltd has accumulated lots of experiences over forty years in this field. During forty years, hundreds of management elites and high science and technology talents were employed.They participated in every walk of the company life, which make our company keep blooming and invincible in the competitive market.

 

Based on the principle of “first quality, sincere service”, our managing ideology is pursuing technology innovation and creating the top brand in the alloy field. We persist in Quality - the foundation of the survival. It is our forever ideology to serve you with full heart and soul. We committed to provide customers all over the world with high-quality, competitive products and perfect service.

 

Our products, such us nichrome wire, nichrome strip, fecral wire, fecral strip, thermocouple wire, nickel wire, nickel strip have been exported to Europe, USA, India, Southest Asia, South America,etc.

We are willing to establish strong and long-time partnership with our customers

  • Most complete range of products dedicated to Resistance, Thermocouple and Furnace manufacturers
  • Quality with end to end production control
  • Technical support and Customer Service
Send your message to this supplier
*From:
Your email address is incorrect!
*To:

Shanghai Tankii Alloy Material Co.,Ltd

*Subject:
Your subject must be between 10-255 characters!
*Message:
Your message must be between 20-3,000 characters!
Characters Remaining : (0/3000)

You May Like

China White Colour Al2O3 Porous Alumina Tube Wear Resisting High Insulation wholesale

White Colour Al2O3 Porous Alumina Tube Wear Resisting High Insulation

China Inconel 601 High Temp Alloy Corrosion Resistant Ncf601 Round Bar Bright Surface wholesale

Inconel 601 High Temp Alloy Corrosion Resistant Ncf601 Round Bar Bright Surface

China Ni29co18/ Uns K94610 (4J29) Kovar Expansion Precision Alloy Pipe / Tube wholesale

Ni29co18/ Uns K94610 (4J29) Kovar Expansion Precision Alloy Pipe / Tube

China Resistohm 80 Ni80cr20 High Temp Alloy For Electric Heating Elements wholesale

Resistohm 80 Ni80cr20 High Temp Alloy For Electric Heating Elements

China High Temperature Refractory 3.8 Alumina Ceramic Roller Tube wholesale

High Temperature Refractory 3.8 Alumina Ceramic Roller Tube

China Thermal Insulation Ceramic Protection Tube High Temp Alloy wholesale

Thermal Insulation Ceramic Protection Tube High Temp Alloy

China High Temperature Furnace 99.97% Alumina Ceramic Tube wholesale

High Temperature Furnace 99.97% Alumina Ceramic Tube

China Alumina 99.7% 99 Al2O3 Insulator Cordierite Ceramic Tube wholesale

Alumina 99.7% 99 Al2O3 Insulator Cordierite Ceramic Tube

China Alumina Ceramic Tube 99.7% 99 Al2O3 High Temp Alloy wholesale

Alumina Ceramic Tube 99.7% 99 Al2O3 High Temp Alloy

China Ni19Mn7 Ni34 Thermal Bimetal High Temp Alloy For Mechanical Work wholesale

Ni19Mn7 Ni34 Thermal Bimetal High Temp Alloy For Mechanical Work

China C70400 C70600 CuNi19 Nickel Silver Strip Hot Rolled Corrosion Resistance wholesale

C70400 C70600 CuNi19 Nickel Silver Strip Hot Rolled Corrosion Resistance

Inquiry Cart 0